摘要
Atmospheric plasma spraying (APS) was used to fabricate 8YSZ (6-8 wt% Y2O3-ZrO2) series coatings with different spraying parameters. Effects of spraying power and powder feed distance on the microstructure, performance and CMAS (calcium-magnesium-alumino-silicate) corrosion resistance of thermal barrier coatings (TBCs) is investigated. The application of coatings at higher spraying powers resulted in enhanced thermal conductivity, hardness, and elastic modulus. It is noteworthy that coatings sprayed at 39-40 kW displayed the highest thermal cycling-CMAS lifetime and CMAS penetration depth. Additionally, a series of embedded micro-aggregated particles (EMAP) coatings was created using different powder feed distances. The porosity of EMAP coatings was significantly higher than that of conventional YSZ coatings, with the EMAP coating produced at a 30 mm powder feed distance showing the highest porosity—approximately 2.5 times greater than that of traditional YSZ coatings. Compared to conventional YSZ coatings, the thermal cycling-CMAS lifetime for the coatings with 30 mm and 40 mm powder feed distances improved by 30% and 55%, respectively. This enhancement is attributed to the increased porosity, which boosts the strain tolerance of the coatings. However, the higher porosity also facilitates CMAS penetration, accelerating the corrosion rate. Therefore, optimizing porosity within the coatings is crucial for enhancing the lifetime and CMAS resistance of TBCs.
 
关键字
Keywords: Thermal barrier coatings; Thermal cycling-CMAS lifetime; Failure behavior; porosity
报告人
Wenkang Zhang
research assistant East China University of Science and Technology, China

稿件作者
Wenkang Zhang 华东理工大学
Weize Wang 华东理工大学
Kaibin Li 华东理工大学
Yangguang Liu 华东理工大学
发表评论
验证码 看不清楚,更换一张
全部评论
段金弟:13971036507  
蒋 超:18971299299 邮箱:icse2024@126.com
李昱鹏:15842490631  
车宏龙:13555943451  
刘明明:19862516876, 邮箱:mmliu@sdut.edu.cn
朱   建:15810878528, 邮箱:zhujian@sdut.edu.cn
张秀丽:15064351998, 邮箱:zhangxiulli@163.com
郭前建:13969397001,  
注册参会 提交稿件